Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 A3K BASF USA
Ultramid®
Electrical field,Electronic field,Industrial machinery,Industrial applications,Non specific food applications
High mobility,Oil resistant
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | BASF USA/A3K |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 75.0 °C |
Melting temperature | ISO 3146 | 260 °C |
mechanical properties | Test Condition | Test Method | BASF USA/A3K |
---|---|---|---|
Bending modulus | 23°C | ISO 178 | 2900 Mpa |
bending strength | 23°C | ISO 178 | 100 Mpa |
Nominal tensile fracture strain | 23°C | ISO 527-2 | 20 % |
Tensile modulus | 23°C | ISO 527-2 | 3000 Mpa |
Tensile strain | Yield,23°C | ISO 527-2 | 5.0 % |
tensile strength | Yield,23°C | ISO 527-2 | 85.0 Mpa |
Physical properties | Test Condition | Test Method | BASF USA/A3K |
---|---|---|---|
density | ISO 1183 | 1.13 g/cm³ | |
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 2.8 % |
Saturation,23°C | ISO 62 | 8.5 % |
impact performance | Test Condition | Test Method | BASF USA/A3K |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 5.0 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180 | 5.5 kJ/m² |
Impact strength of simply supported beam without notch | -30°C | ISO 179 | NoBreak |
23°C | ISO 179 | NoBreak |