Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/NH-1904 BK |
|---|---|---|---|
| elongation | Break | ASTM D638 | 15 % |
| bending strength | ISO 178 | 68.0 Mpa | |
| tensile strength | Break | ASTM D638 | 40.0 Mpa |
| Tensile strain | Break | ISO 527-2/5 | 15 % |
| tensile strength | Yield | ASTM D638 | 41.0 Mpa |
| Bending modulus | ASTM D790 | 2400 Mpa | |
| tensile strength | Yield | ISO 527-2/5 | 45.0 Mpa |
| Tensile modulus | ISO 527-2/5 | 2300 Mpa | |
| Bending modulus | ISO 178 | 2700 Mpa | |
| bending strength | ASTM D790 | 66.0 Mpa | |
| Tensile modulus | ASTM D638 | 2200 Mpa | |
| tensile strength | Break | ISO 527-2/5 | 44.0 Mpa |
| impact performance | Test Condition | Test Method | Samsung Cheil South Korea/NH-1904 BK |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 7.0 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 7.0 kJ/m² |
| thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/NH-1904 BK |
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 79.0 °C |
| 1.8MPa,Unannealed,4.00mm | ISO 75-2/A | 72.0 °C | |
| Vicat softening temperature | ISO 306/B50 | 94.0 °C | |
| flammability | Test Condition | Test Method | Samsung Cheil South Korea/NH-1904 BK |
| UL flame retardant rating | 2.5mm | UL 94 | V-0 |
| 1.5mm | UL 94 | V-1 | |
| Physical properties | Test Condition | Test Method | Samsung Cheil South Korea/NH-1904 BK |
| Shrinkage rate | MD:3.20mm | ISO 2577 | 0.40-0.70 % |
| melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 44 g/10min |
| Shrinkage rate | MD:3.20mm | ASTM D955 | 0.40-0.70 % |
| melt mass-flow rate | 220°C/10.0kg | ASTM D1238 | 44 g/10min |