Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Color
Grade
Reference Price
| Physical properties | Test Condition | Test Method | HENGLI DALIAN/HLGP850 |
|---|---|---|---|
| styrene content | GB/T 16867-1997 | 330 mg/kg | |
| melt mass-flow rate | GB/T 3682.1-2018 | 8.1 g/10min | |
| Particle appearance, black particles | 0 个/kg | ||
| Impurities and color particles | 0 个/kg | ||
| Shrinkage rate | GB/T 17037.4-2003 | 0.5 % | |
| mechanical properties | Test Condition | Test Method | HENGLI DALIAN/HLGP850 |
| Charpy Notched Impact Strength | GB/T 1043.1-2008 | 8 kJ/㎡ | |
| Tensile stress | Break | GB/T 1040 | 48.5 Mpa |
| thermal performance | Test Condition | Test Method | HENGLI DALIAN/HLGP850 |
| Vicat softening temperature | GB/T 1633-2000 | 96 ℃ | |
| Hot deformation temperature | 1.8MPa | GB/T 1634.2-2019 | 89 ℃ |
| optical performance | Test Condition | Test Method | HENGLI DALIAN/HLGP850 |
| Transmittance rate | GB/T 2410-2008 | 90 % |