PC HF1110R SABIC INNOVATIVE NANSHA
LEXAN™ 
Thin walled products,lens,Optical data storage,Safety equipment,container
High mobility,Good demolding performanc,Good forming performance
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
Hot deformation temperature1.8 MPa, Unannealed, 3.20 mmASTM D648126 °C
RTIUL 746130 °C
RTI ElecUL 746130 °C
RTI ImpUL 746130 °C
mechanical propertiesTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
Bending modulus50.0 mm SpanASTM D7902300 Mpa
bending strengthYield, 50.0 mm SpanASTM D79093.0 Mpa
elongationBreakASTM D638120 %
tensile strengthYieldASTM D63862.0 Mpa
BreakASTM D63865.0 Mpa
Electrical performanceTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
Compared to the anti leakage trace indexUL 746PLC 2
High arc combustion indexUL 746PLC 1
High voltage arc tracing rateUL 746PLC 2
Hot wire ignitionUL 746PLC 2
Physical propertiesTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
melt mass-flow rate300°C/1.2 kgASTM D123825 g/10 min
Shrinkage rate3.20 mm,FlowInternal Method0.50 - 0.70 %
impact performanceTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
Dart impact23°C, Energy at PeakASTM D376354.0 J
Impact strength of cantilever beam gapASTM D1822378 kJ/m²
flammabilityTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
UL flame retardant rating1.1 mmUL 94V-2
optical performanceTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
transmissivity2540 μmASTM D100388.0 %
turbidity2540 μmASTM D10031.0 %
injectionTest ConditionTest MethodSABIC INNOVATIVE NANSHA/HF1110R
Back pressure0.300 to 0.700 Mpa
drying temperature120 °C
drying time3.0 to 4.0 hr
Exhaust hole depth0.025 to 0.076 mm
Mold temperature70 to 95 °C
Processing (melt) temperature270 to 295 °C
Screw speed40 to 70 rpm
Spray nozzle temperature265 to 290 °C
Suggested injection volume40 to 60 %
Suggested maximum moisture content0.020 %
Temperature at the front of the material cylinder270 to 295 °C
Temperature at the rear of the barrel250 to 270 °C
Temperature in the middle of the barrel260 to 280 °C