PA6 6G25VOP DOMO CHEM GERMANY
--
--
Filler: Glass fiber reinf、25% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | DOMO CHEM GERMANY/6G25VOP |
---|---|---|---|
Rockwell hardness | R级 | ISO 2039-2 | 120 |
Mechanical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6G25VOP |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 8500 Mpa | |
tensile strength | 断裂 | ISO 527-2/5 | 125 Mpa |
Tensile strain | 断裂 | ISO 527-2/5 | 2.5 % |
Electrical performance | Test Condition | Test Method | DOMO CHEM GERMANY/6G25VOP |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+15 ohms·cm | |
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | V |
Surface Resistivity | IEC 60093 | 1E+13 ohms |
flammability | Test Condition | Test Method | DOMO CHEM GERMANY/6G25VOP |
---|---|---|---|
burning rate | FMVSS302 | <100 mm/min | |
Burning wire flammability index | 1.0到3.0mm | IEC 60695-2-12 | 960 °C |
UL flame retardant rating | 0.8mm | UL 94 | V-0 |
physical property | Test Condition | Test Method | DOMO CHEM GERMANY/6G25VOP |
---|---|---|---|
Water absorption rate | 饱和,23°C | ISO 62 | 5.0 % |
Shrinkage rate | MD2:23°C,72小时 | ISO 2577 | 0.20-0.40 % |
Thermal performance | Test Condition | Test Method | DOMO CHEM GERMANY/6G25VOP |
---|---|---|---|
melting temperature | ISO 11357-3 | 218to222 °C | |
Hot deformation temperature (HDT) | 1.8MPa,未退火,HDT | ISO 75-2/A | 190 °C |
vicat | ISO 306/B50 | 210 °C | |
Hot deformation temperature (HDT) | 0.45MPa,未退火,HDT | ISO 75-2/B | 210 °C |