ABS GP-25 INEOS STYRO KOREA
Terluran®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | INEOS STYRO KOREA/GP-25 |
---|---|---|---|
elongation at break | 屈服,23°C | ISO 527-2 | 2.4 % |
Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 7 kJ/m² |
23°C | ISO 179/1eA | 19 kJ/m² | |
tensile strength | 屈服,23°C | ISO 527-2 | 44 Mpa |
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 22 kJ/m² |
Tensile modulus | 23°C | ISO 527-2 | 2300 Mpa |
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 90 kJ/m² |
elongation at break | 23°C | ISO 527-2 | 12 % |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 125 kJ/m² |
Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 7 kJ/m² |
Electrical performance | Test Condition | Test Method | INEOS STYRO KOREA/GP-25 |
---|---|---|---|
Volume resistivity | IEC 60093 | >=1.0E+15 Ω.cm |
optical performance | Test Condition | Test Method | INEOS STYRO KOREA/GP-25 |
---|---|---|---|
Yellowness Index | DIN 6167 | 15 YI |
Flame retardancy | Test Condition | Test Method | INEOS STYRO KOREA/GP-25 |
---|---|---|---|
UL flame retardant rating | Allcolor | UL -94 | HB 3.00mm |
Allcolor | UL -94 | HB 1.50mm |
physical property | Test Condition | Test Method | INEOS STYRO KOREA/GP-25 |
---|---|---|---|
Shrinkage rate | MD2.0mm | ISO 294-4 | 0.4 % |
Water absorption rate | 23°C,24hr | ISO 62 | 0.21 % |
23°C,50RH | ISO 62 | 0.95 % | |
Shrinkage rate | TD2.0mm | ISO 294-4 | 0.7 % |
melt mass-flow rate | 220℃/10Kg | ISO 1133 | 25 g/10min |
Thermal performance | Test Condition | Test Method | INEOS STYRO KOREA/GP-25 |
---|---|---|---|
melting temperature | ISO 11357-3 | 220-260 °C | |
thermal conductivity | DIN 52612 | 0.170 W/m/K | |
Heat distortion temperature | 1.80MPa未退火,HDT | ISO 75-2/Af | 93 °C |
vicat | 5.1kg | ISO 306/A50 | 95 °C |
1.02kg | ISO 306/B50 | 103 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 8.0E-5 cm/cm/°C |
Heat distortion temperature | 0.45MPa未退火,HDT | ISO 75-2/Bf | 97 °C |