Basic performance | Test Condition | Test Method | USA Suwei/A-701 |
---|---|---|---|
melt mass-flow rate | 343℃/2.16 kg | ASTM D1238 | 70 g/10 min |
density | ASTM D792 | 1.37 g/cm³ | |
Water absorption rate | 24hr | ASTM D570 | 0.54 % |
Shrinkage rate | flow | ASTM D955 | 0.60 % |
Electrical performance | Test Condition | Test Method | USA Suwei/A-701 |
---|---|---|---|
dielectric constant | 1000 Hz | ASTM D150 | 3.50 |
Dielectric loss | 60 Hz | ASTM D150 | 0.0017 |
Volume resistivity | ASTM D257 | 1.7E+15 ohm·cm | |
dielectric strength | ASTM D149 | 15 kV/mm | |
Dielectric loss | 1000 Hz | ASTM D150 | 0.0022 |
dielectric constant | 1E+6 Hz | ASTM D150 | 3.54 |
60 Hz | ASTM D150 | 3.51 | |
Dielectric loss | 1E+6 Hz | ASTM D150 | 0.0056 |
Mechanical properties | Test Condition | Test Method | USA Suwei/A-701 |
---|---|---|---|
elongation | Break | ASTM D638 | 30 % |
Yield | ASTM D638 | 6.5 % | |
Suspended wall beam without notch impact strength | ASTM D256 | 69.4 J/m | |
Tensile modulus | ASTM D638 | 2650 MPa | |
Flexural modulus | ASTM D790 | 2900 MPa | |
tensile strength | Break | ASTM D638 | 82.7 MPa |
bending strength | ASTM D790 | 111 MPa |
Thermal performance | Test Condition | Test Method | USA Suwei/A-701 |
---|---|---|---|
Linear coefficient of thermal expansion | flow | ASTM D696 | 0.000049 cm/cm/°C |
Heat distortion temperature | 1.8Mpa,未退火,HDT | ASTM D648 | 202 ℃ |