Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC K-1300 TEIJIN JAPAN
PANLITE®
film、Pipeline components
wear resistant、Toughening、Low temperature resistanc、High impact resistance、high viscosity
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical Properties | Test Condition | Test Method | TEIJIN JAPAN/K-1300 |
---|---|---|---|
Tensile Elongation?(Break) | ASTM D638/ISO 527 | 130 % | |
Rockwell Hardness | ASTM D785 | 77 | |
Tensile Elongation | ASTM D638/ISO 527 | 6 % | |
Flexural Modulus | ASTM D790/ISO 178 | 2190(22300) kg/cm²(MPa)[Lb/in²] |
Other | Test Condition | Test Method | TEIJIN JAPAN/K-1300 |
---|---|---|---|
purpose | 用途:薄板、薄膜、管子等的挤出成型品。・各种瓶类的直接吹塑成型品。・大型容器等的回转熔塑成型品。 | ||
characteristic | 特性:高粘度、挤塑、吹塑及注塑成型、力学性能好 |
Optical | Test Condition | Test Method | TEIJIN JAPAN/K-1300 |
---|---|---|---|
Index of Refraction | ASTM D542/ISO 489 | 1.585 | |
Transmittance | ASTM D1003/ISO 13468 | 89 % |
Physical Properties | Test Condition | Test Method | TEIJIN JAPAN/K-1300 |
---|---|---|---|
Density | ASTM D792/ISO 1183 | 1.20 | |
Modeling Shrinkage | ASTM D955 | 0.5~0.7 % |
Electrical Properties | Test Condition | Test Method | TEIJIN JAPAN/K-1300 |
---|---|---|---|
Volume Resistivity | ASTM D257/IEC 60093 | 3 Ω.cm |
Contact Us
Get App
Top