PPO(PPE)+TPE NORYL™ WCD795 resin SABIC
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | SABIC/NORYL™ WCD795 resin |
---|---|---|---|
Shore hardness | 邵氏A,30秒 | ASTM D2240 | 79 |
Mechanical properties | Test Condition | Test Method | SABIC/NORYL™ WCD795 resin |
---|---|---|---|
fracture | ISO 527-2/50 | 14.5 MPa | |
ISO 527-2/50 | 220 % | ||
ASTM D638 | 240 % | ||
ASTM D638 | 14.5 MPa | ||
UL 1581 | 21.5 MPa | ||
UL 1581 | 250 % |
Electrical performance | Test Condition | Test Method | SABIC/NORYL™ WCD795 resin |
---|---|---|---|
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | PLC 0 | |
Volume resistivity | ASTM D257 | 1.4E+16 ohms·cm | |
Dissipation Factor | 1MHz | ASTM D150 | 7E-03 |
dielectric constant | 1MHz | ASTM D150 | 2.60 |
dielectric strength | 2.00mm,在油中 | IEC 60243-1 | 25 kV/mm |
flammability | Test Condition | Test Method | SABIC/NORYL™ WCD795 resin |
---|---|---|---|
Smoke density | Non-Flame,0.5mmplaque,Ds,max | ASTME662 | 70 |
VW | UL 1581 | Pass | |
Hot filament ignition temperature | 3.00mm | IEC 60695-2-13 | 800 °C |
Burning wire flammability index | 3.00mm | IEC 60695-2-12 | 960 °C |
Smoke density | Flame,0.5mmplaque,Ds,max | ASTME662 | 120 |
Limiting Oxygen Index | ISO 4589-2 | 27 % |
physical property | Test Condition | Test Method | SABIC/NORYL™ WCD795 resin |
---|---|---|---|
density | ASTM D792 | 1.02 g/cm³ | |
melt mass-flow rate | 250°C/10.0kg | ASTM D1238 | 11 g/10min |
Thermal performance | Test Condition | Test Method | SABIC/NORYL™ WCD795 resin |
---|---|---|---|
Heat distortion temperature | 121°C | UL 1581 | 8.0 % |
brittle temperature | ASTM D746 | <-40.0 °C |