Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC/ABS LG8002 SABIC INNOVATIVE US
CYCOLAC™ 
Automotive sector
Low gloss,developable ,High impact
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Electrical performanceTest ConditionTest MethodSABIC INNOVATIVE US/LG8002
Surface ResistivityASTM D257/IEC 60093-- Ω
dielectric constantASTM D150/IEC 60250--
arc resistanceASTM D495/IEC 60112--
Volume resistivityASTM D257/IEC 60093-- Ω.cm
Mechanical propertiesTest ConditionTest MethodSABIC INNOVATIVE US/LG8002
Impact strength of cantilever beam gapASTM D256/ISO 179-- kg·cm/cm(J/M)ft·lb/in
bending strengthASTM D790/ISO 178870 kg/cm²(MPa)[Lb/in²]
Flexural modulusASTM D790/ISO 17823200 kg/cm²(MPa)[Lb/in²]
elongationASTM D638/ISO 5275.0 %
Tensile modulusASTM D638/ISO 527-- kg/cm²(MPa)[Lb/in²]
Charpy Notched Impact StrengthASTM D256/ISO 179-- kg·cm/cm(J/M)ft·lb/in
elongation at breakASTM D638/ISO 527120 %
Rockwell hardnessASTM D785--
tensile strength ASTM D638/ISO 527560 kg/cm²(MPa)[Lb/in²]
otherTest ConditionTest MethodSABIC INNOVATIVE US/LG8002
characteristic低光泽.高冲击.延展性.紫外线稳定。适用于:汽车
notes注射成型
Color本色
Physical propertiesTest ConditionTest MethodSABIC INNOVATIVE US/LG8002
Shrinkage rateASTM D9550.50-0.70 %
densityASTM D792/ISO 11831.13
melt mass-flow rateASTM D1238/ISO 1133-- g/10min
Water absorption rateASTM D570/ISO 62-- %
Thermal performanceTest ConditionTest MethodSABIC INNOVATIVE US/LG8002
Combustibility (rate)UL 94--
Heat distortion temperatureHDTASTM D648/ISO 750.45MPa/3.20mm.121℃;1.80MPa/3.20mm.104℃ ℃(℉)
vicatASTM D1525/ISO R306-- ℃(℉)
Linear coefficient of thermal expansionASTM D696/ISO 113590.000090 mm/mm.℃

Contact Us