Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA/MXD6 1022H BK MITSUBISHI ENGINEERING JAPAN
RENY™
Automotive sector,Electronic field,Electrical field
Glass fiber reinforced,Filler: Glass fiber reinf,50% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/1022H BK |
---|---|---|---|
0.45MPa, unannealed | °C | 234to255 | |
1.8MPa, unannealed | °C | 223to230 | |
flow | mm/mm/°C | 137.2E-5-25.4E-5 | |
transverse | mm/mm/°C | 55.9E-5-50.8E-5 |
mechanical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/1022H BK |
---|---|---|---|
Fracture, 23 ℃ | 151.72to280.69 MPa | ||
% | 1.6to2.1 | ||
Yield, 23 ℃ | % | 2.0to3.0 |
Electrical performance | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/1022H BK |
---|---|---|---|
Compared to the anti leakage trace index | V | ||
Dielectric strength | 23℃ | V/mil | 500to840 |
Surface resistivity | ohms | 5.0E+3-6.0E+15 | |
Volume resistivity | 23℃ | ohms·cm | 3.0E+2-2.1E+16 |
Physical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/1022H BK |
---|---|---|---|
23℃,24hr | % | 0.16to0.30 | |
Balance, 23 ℃, 50% RH | % | 0.70to1.5 | |
Flow: 23 ℃ | Flow,23℃ | mm/mm | 38.1E-3-78.7E-3 |
melt mass-flow rate | 275°C/2.16kg | g/10min | 3.6to20 |
Melt Volume Flow Rate (MVR) | 275°C/2.16kg | ISO 527-2/5 | 0.01to0.04 |
Saturation, 23 ℃ | % | 0.060to0.15 |
impact performance | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/1022H BK |
---|---|---|---|
Impact strength of simply supported beam without notch | 23℃ | kJ/m² | 2.647to20.893 |
Suspended wall beam without notch impact strength | 23℃ | J/m | 0.222to0.332 |
flammability | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/1022H BK |
---|---|---|---|
Hot filament ignition temperature | °C | 798to904 |