Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC 141R-111 SABIC INNOVATIVE US
LEXAN™
--
transparent,Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic Performance | Test Condition | Test Method | SABIC INNOVATIVE US/141R-111 |
---|---|---|---|
melt mass-flow rate | ASTM D-1238 | 10.5 g/10min |
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/141R-111 |
---|---|---|---|
Hot deformation temperature | 1.8MPa | ASTM D-648 | 132 °C |
0.45MPa | ASTM D-648 | 137 °C | |
Linear coefficient of thermal expansion | E831 | 6.8×10 1/°C | |
Long term use temperature | UL 746B | 130 °C | |
UL flame retardant rating | UL 94 | 1.1 mm | |
UL94 | HB | ||
Vicat softening temperature | ASTM D-1525 | 154 °C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/141R-111 |
---|---|---|---|
Bending modulus | ASTM D-790 | 2343 Mpa | |
bending strength | ASTM D-790 | 96 Mpa | |
Elongation at Break | Break点 | ASTM D-638 | 130 % |
Impact strength of cantilever beam gap | Notched23°C | ASTM D-256 | 800 J/m |
Rockwell hardness | R | ASTM D-785 | 118 |
tensile strength | Break点 | ASTM D-638 | 69 Mpa |
屈伏点 | ASTM D-638 | 62 Mpa |
Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/141R-111 |
---|---|---|---|
Dielectric constant | 1MHz | ASTM D-150 | 2.96 |
60Hz | ASTM D-150 | 3.17 | |
Dissipation factor | 1MHz | ASTM D-150 | 0.01 |
60Hz | ASTM D-150 | 0.0009 | |
Volume resistivity | ASTM D-257 | 1.0×10 ohm-cm |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/141R-111 |
---|---|---|---|
density | ASTM D-792 | 1.2 | |
Shrinkage rate | 3.2mm | ASTM D-955 | 5-7 10 |
Water absorption rate | % | ASTM D-570 | 0.15 |