Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PUR-Ester Witcobond® A-100 CHEMTURU USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | CHEMTURU USA/Witcobond® A-100 |
---|---|---|---|
Shore hardness | 64.0 | ||
Hardness | 3H |
thermosetting | Test Condition | Test Method | CHEMTURU USA/Witcobond® A-100 |
---|---|---|---|
Thermosetting mixed viscosity | 25°C | 5.00to100 cP |
physical property | Test Condition | Test Method | CHEMTURU USA/Witcobond® A-100 |
---|---|---|---|
Solid Content | 34to36 % | ||
density | 1.05 g/cm³ | ||
pH value | 25°C | 7.0to9.0 |
elastomer | Test Condition | Test Method | CHEMTURU USA/Witcobond® A-100 |
---|---|---|---|
tensile strength | 100%应变 | 44.8 MPa | |
elongation | 断裂 | 140 % | |
tensile strength | 49.6 MPa |
Thermal performance | Test Condition | Test Method | CHEMTURU USA/Witcobond® A-100 |
---|---|---|---|
Glass Transition Temperature | 77.0 °C |