Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA46 TW271B6 DSM HOLAND
Stanyl® 
Home appliance components、Electronic and electrical
Thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodDSM HOLAND/TW271B6
Charpy Notched Impact Strength23°CISO 179/1eA7.0 kJ/m²
-30°CISO 179/1eA7.0 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU50 kJ/m²
-30°CISO 179/1eU50 kJ/m²
Mechanical propertiesTest ConditionTest MethodDSM HOLAND/TW271B6
tensile strength 断裂, 160°CISO 527-2115 Mpa
Tensile modulus--ISO 527-224000 Mpa
tensile strength 断裂, 180°CISO 527-2105 Mpa
Tensile strain断裂, 120°CISO 527-23.1 %
tensile strength 断裂ISO 527-2260 Mpa
Tensile modulus180°CISO 527-211500 Mpa
tensile strength 断裂, 120°CISO 527-2140 Mpa
Tensile modulus160°CISO 527-212000 Mpa
120°CISO 527-213500 Mpa
Tensile strain断裂, 200°CISO 527-23.1 %
断裂, 180°CISO 527-23.1 %
断裂ISO 527-21.7 %
断裂, 160°CISO 527-23.1 %
Tensile modulus200°CISO 527-211000 Mpa
tensile strength 断裂, 200°CISO 527-295.0 Mpa
physical property Test ConditionTest MethodDSM HOLAND/TW271B6
Water absorption rate平衡, 23°C, 50% RHISO 622.4 %
densityISO 11831.32 g/cm³
Shrinkage rate流量ISO 294-40.30 %
横向流量ISO 294-40.70 %
Thermal performanceTest ConditionTest MethodDSM HOLAND/TW271B6
melting temperatureISO 11357-3295 °C
Heat distortion temperature1.8 MPa, 未退火,HDTISO 75-2/A290 °C
Linear coefficient of thermal expansion流动ISO 11359-22.5E-5 cm/cm/°C
横向ISO 11359-23.5E-5 cm/cm/°C