PP Resblend PP/PA Polimarky Spolka Jawna
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| mechanical properties | Test Condition | Test Method | Polimarky Spolka Jawna/Resblend PP/PA |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 2500to3300 MPa | |
| Tensile strain | Break | ISO 527-2 | 40to55 % |
| tensile strength | ISO 527-2 | 39.0to42.0 MPa |
| Physical properties | Test Condition | Test Method | Polimarky Spolka Jawna/Resblend PP/PA |
|---|---|---|---|
| density | ISO 1183 | 0.960to1.05 g/cm³ |
| impact performance | Test Condition | Test Method | Polimarky Spolka Jawna/Resblend PP/PA |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1A | 3.5to5.5 kJ/m² |