Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU 385A COVESTRO GERMANY
Desmopan®
film、Architectural application、Profile、currency、pipeline、Profile、Engineering accessories
wear resistant、Chemical resistance、High temperature resistan、currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Elastomers Properties | Test Condition | Test Method | COVESTRO GERMANY/385A |
---|---|---|---|
Tearing Strength | 23°C | ISO34-1 | 70 kN/m |
Compression Set | 23°C,72hr | ISO815 | 15 % |
70°C,24hr | ISO815 | 42 % |
Hardness | Test Condition | Test Method | COVESTRO GERMANY/385A |
---|---|---|---|
Shore Hardness | 邵氏D,15秒 | ISO8682 | 33 |
邵氏A,3秒 | ISO8682 | 85 |
Mechanical Properties | Test Condition | Test Method | COVESTRO GERMANY/385A |
---|---|---|---|
Tensile Strength | Break,23°C | DIN53504 | 52.0 Mpa |
Tensile Stress | 100%应变,23°C | DIN53504 | 5.80 Mpa |
50%应变,23°C | ISO527-3 | 4.70 Mpa | |
Abrasion Resistance | 23°C | ISO4649-A | 25.0 mm³ |
Tensile Stress | 10%应变,23°C | ISO527-3 | 2.00 Mpa |
Tensile Modulus | -20°C | ISO6721-1,-4 | 84.0 Mpa |
Tensile Stress | 300%应变,23°C | DIN53504 | 16.6 Mpa |
Tensile Strain | 断裂,23°C | DIN53504 | 530 % |
Tensile Modulus | 20°C | ISO6721-1,-4 | 28.0 Mpa |
60°C | ISO6721-1,-4 | 21.0 Mpa |
Impact Properties | Test Condition | Test Method | COVESTRO GERMANY/385A |
---|---|---|---|
ImpactResilience | 23°C | ISO4662 | 50 % |