Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC/ABS 8260H KUMHO KOREA
--
Phone,Shell
High impact resistance,High mobility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | KUMHO KOREA/8260H |
---|---|---|---|
CSAFileNo | LS66457 |
thermal performance | Test Condition | Test Method | KUMHO KOREA/8260H |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 106 °C |
Vicat softening temperature | ASTM D15252 | 118 °C |
mechanical properties | Test Condition | Test Method | KUMHO KOREA/8260H |
---|---|---|---|
Bending modulus | ASTM D790 | 2100 Mpa | |
bending strength | ASTM D790 | 80.0 Mpa | |
elongation | Break | ASTM D638 | 100 % |
tensile strength | ASTM D638 | 56.0 Mpa |
Electrical performance | Test Condition | Test Method | KUMHO KOREA/8260H |
---|---|---|---|
Surface resistivity | IEC 60093 | >1.0E+15 ohms | |
Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm |
Physical properties | Test Condition | Test Method | KUMHO KOREA/8260H |
---|---|---|---|
melt mass-flow rate | 230°C/10.0kg | ASTM D1238 | 25 g/10min |
Shrinkage rate | MD | ASTM D955 | 0.50-0.70 % |
flammability | Test Condition | Test Method | KUMHO KOREA/8260H |
---|---|---|---|
UL flame retardant rating | 1.6mm | UL 94 | HB |