Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA6 Nylux 6/G33FL BLK KMI Group, Inc.
--
--
Filler, glass fiber reinforced material, 33%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodKMI Group, Inc./Nylux 6/G33FL BLK
Rockwell hardnessISO 2039-2122 R
Mechanical propertiesTest ConditionTest MethodKMI Group, Inc./Nylux 6/G33FL BLK
Flexural modulus23°CISO 1785800 MPa
Tensile modulus23°CISO 527-28500 MPa
Impact strength of cantilever beam gap23°CISO 180/1A5 kJ/m²
tensile strength 23°CISO 527-2140 MPa
elongation at break23°CISO 527-23 %
Electrical performanceTest ConditionTest MethodKMI Group, Inc./Nylux 6/G33FL BLK
Surface ResistivityIEC 600931E+13 Ω.cm
Volume resistivityIEC 600931E+15 Ω.cm
Flame retardant performanceTest ConditionTest MethodKMI Group, Inc./Nylux 6/G33FL BLK
UL flame retardant ratingUL -94HB 0.8mm
physical property Test ConditionTest MethodKMI Group, Inc./Nylux 6/G33FL BLK
Water absorption rate(23°C,24hr)ISO 626.0 %
densityISO 11831.36 g/cm³
Water absorption rate收缩率ISO 25770.25-0.55 %
Thermal performanceTest ConditionTest MethodKMI Group, Inc./Nylux 6/G33FL BLK
vicatISO 306/A50210 °C
Heat distortion temperature1.80MPa退火,HDTISO 75-2/Af205 °C
Linear coefficient of thermal expansion熔融温度ISO 3146220 °C
Heat distortion temperature0.45MPa未退火,HDTISO 75-2/Bf215 °C

Contact Us