| mechanical properties | Test Condition | Test Method | LUBRIZOL USA/58252 |
|---|---|---|---|
| tensile strength | Break | ASTM D-412 | 9.00 Mpa |
| Tensile stress | 400% Strain | ASTM D-412 | 6.70 Mpa |
| tensile strength | 100%Strain | ASTM D-412 | 6.21 Mpa |
| Taber abraser | 1000 Cycles, 1000 g, H-18 Wheel | ASTM D-3389 | 140 mg |
| elongation | Break | ASTM D-412 | 800 % |
| Stretch permanent deformation | 200% Strain | ASTM D-412 | 7 % |
| tear strength | -- 4 | ASTM D-624 | 47.3 kN/m |
| Water vapor permeability | ASTM E96 | 850 g/m²/24 hr | |
| thermal performance | Test Condition | Test Method | LUBRIZOL USA/58252 |
| Glass transition temperature | DSC | Internal Method | -28.0 °C |
| Melting temperature | Internal Method | 130 °C | |
| Vicat softening temperature | Internal Method | 47.0 °C | |
| Physical properties | Test Condition | Test Method | LUBRIZOL USA/58252 |
| Shore hardness | Shore A | ASTM D-2240 | 70 |