Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PCTG MX711 EASTMAN USA
Tritan™
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | EASTMAN USA/MX711 |
---|---|---|---|
Dart impact | -40°C,EnergyatPeakLoad | ASTM D3763 | 66.0 J |
23°C,EnergyatPeakLoad | ASTM D3763 | 61.0 J |
hardness | Test Condition | Test Method | EASTMAN USA/MX711 |
---|---|---|---|
Rockwell hardness | R计秤,23°C | ASTM D785 | 112 |
Mechanical properties | Test Condition | Test Method | EASTMAN USA/MX711 |
---|---|---|---|
Tensile modulus | 23°C | ASTM D638 | 1550 Mpa |
23°C | ISO 527-2 | 1550 Mpa | |
tensile strength | 断裂,23°C | ISO 527-2 | 58.0 Mpa |
屈服,23°C | ASTM D638 | 43.0 Mpa | |
断裂,23°C | ASTM D638 | 53.0 Mpa | |
Tensile strain | 断裂,23°C | ISO 527-2 | 190 % |
bending strength | 23°C | ISO 178 | 59.0 Mpa |
tensile strength | 屈服,23°C | ISO 527-2 | 43.0 Mpa |
Tensile strain | 屈服,23°C | ISO 527-2 | 7.0 % |
Flexural modulus | 23°C | ISO 178 | 1500 Mpa |
elongation | 屈服,23°C | ASTM D638 | 6.0 % |
bending strength | 屈服,23°C | ASTM D790 | 62.0 Mpa |
Flexural modulus | 23°C | ASTM D790 | 1550 Mpa |
elongation | 断裂,23°C | ASTM D638 | 210 % |
optical performance | Test Condition | Test Method | EASTMAN USA/MX711 |
---|---|---|---|
transmissivity | 总计 | ASTM D1003 | 90.0 % |
Haze ratio | ASTM D1003 | <1.0 % |
physical property | Test Condition | Test Method | EASTMAN USA/MX711 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.50-0.70 % |
Thermal performance | Test Condition | Test Method | EASTMAN USA/MX711 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 85.0 °C |
0.45MPa,未退火,HDT | ASTM D648 | 99.0 °C |