PA6/6T TKR4340G6 LS BK BASF GERMANY
Ultramid®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | BASF GERMANY/TKR4340G6 LS BK |
|---|---|---|---|
| Hot deformation temperature | Unannealed1.8MPa | ISO 75 | 220 °C |
| Linear coefficient of thermal expansion | Flow | ISO 11359 | 2.3E-5 cm/cm/℃ |
| 垂直 | ISO 11359 | 7E-5 cm/cm/℃ | |
| Melting temperature | ISO 11357 | 290 °C | |
| thermal conductivity | DIN 52612 | 0.37 W/(m.K) |
| mechanical properties | Test Condition | Test Method | BASF GERMANY/TKR4340G6 LS BK |
|---|---|---|---|
| bending strength | 23℃ | ISO 178 | 240 Mpa |
| Charpy Notched Impact Strength | 23℃ | ISO 179 | 65 kJ/m² |
| elongation | 23℃ | ISO 527 | 2.5 % |
| Impact strength of simply supported beam without notch | ISO 179 | 8 kJ/m² | |
| Tensile modulus | 23℃ | ISO 527 | 1100 Mpa |
| tensile strength | 23℃ | ISO 527 | 150 Mpa |
| flame retardant performance | Test Condition | Test Method | BASF GERMANY/TKR4340G6 LS BK |
|---|---|---|---|
| UL flame retardant rating | 1.6mm | UL 94 | V-0 |
| Electrical performance | Test Condition | Test Method | BASF GERMANY/TKR4340G6 LS BK |
|---|---|---|---|
| Dielectric constant | 1MHz | IEC 60250 | 0.015 |
| Volume resistivity | IEC 60093 | 1E17 Ω.cm |
| Physical properties | Test Condition | Test Method | BASF GERMANY/TKR4340G6 LS BK |
|---|---|---|---|
| density | ISO 1183 | 1.46 g/cm³ | |
| Shrinkage rate | Flow | ISO 294 | 0.3 % |
| 垂直 | ISO 294 | 0.7 % | |
| smoke index | 5kg | ISO 1133 | 45 cm3/10mir |
| Water absorption rate | 23°C50RH | ISO 62 | 1.6 % |
| 23℃ 24hr | ISO 62 | 4.8 % |