PP Homopolymer NEFTEKHIM PP 1525H (S28F) Nizhnekamskneftekhim Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Nizhnekamskneftekhim Inc./NEFTEKHIM PP 1525H (S28F) |
---|---|---|---|
Rockwell hardness | R级 | 82to95 |
Supplementary Information | Test Condition | Test Method | Nizhnekamskneftekhim Inc./NEFTEKHIM PP 1525H (S28F) |
---|---|---|---|
ThermalCreepTemperature | 90to96 °C | ||
Thermal-oxidativeDeterioration | 150°C | 15.0 day |
Mechanical properties | Test Condition | Test Method | Nizhnekamskneftekhim Inc./NEFTEKHIM PP 1525H (S28F) |
---|---|---|---|
elongation | 屈服 | ASTM D638 | 10 % |
Flexural modulus | ASTM D790 | 1500 MPa | |
tensile strength | 屈服 | ASTM D638 | 34.0 MPa |
physical property | Test Condition | Test Method | Nizhnekamskneftekhim Inc./NEFTEKHIM PP 1525H (S28F) |
---|---|---|---|
Apparent density | 0.48to0.52 g/cm³ | ||
gel content | >2.50mm | 0.00 pcs/m² | |
density | 0.900 g/cm³ | ||
ash content | 0.025to0.050 % | ||
gel content | >200.0µm | 300 pcs/m² | |
melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 1.7to2.3 g/10min |
gel content | 0.700到1.50mm | 3.00 pcs/m² | |
1.50到2.50mm | 0.00 pcs/m² |
Thermal performance | Test Condition | Test Method | Nizhnekamskneftekhim Inc./NEFTEKHIM PP 1525H (S28F) |
---|---|---|---|
vicat | 150to154 °C |