EVOH E105B KURARAY JAPAN
EVAL™
--
Lubricity,copolymer
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | KURARAY JAPAN/E105B |
|---|---|---|---|
| Crystallization peak temperature | DSC | ISO 3146 | 145 °C |
| Glass transition temperature | DSC | DSC | 53.0 °C |
| Melting temperature | ISO 3146 | 165 °C |
| mechanical properties | Test Condition | Test Method | KURARAY JAPAN/E105B |
|---|---|---|---|
| Bending modulus | ISO 178 | 4800 Mpa | |
| Charpy Notched Impact Strength | ISO 179 | 2.0 kJ/m² | |
| Rockwell hardness | M -Sale | ISO 2039-2 | 80 |
| Tensile modulus | ISO 527-2 | 2300 Mpa | |
| Tensile strain | Break | ISO 527-2 | 11 % |
| tensile strength | Break | ISO 527-2 | 29.0 Mpa |
| Physical properties | Test Condition | Test Method | KURARAY JAPAN/E105B |
|---|---|---|---|
| Ethylene component | 44.0 wt% | ||
| melt mass-flow rate | 210℃/2.16 kg | ISO 1133 | 13 g/10 min |
| 190℃/2.16 kg | ISO 1133 | 5.7 g/10 min |