PA6 TAROMID B 280 G2 X2 Taro Plast S.p.A.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Taro Plast S.p.A./TAROMID B 280 G2 X2 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 4.0 kJ/m² |
Impact strength of cantilever beam gap | 23°C,3.20mm | ASTMD256 | 50 J/m |
hardness | Test Condition | Test Method | Taro Plast S.p.A./TAROMID B 280 G2 X2 |
---|---|---|---|
Rockwell hardness | R级 | ASTM D785 | 100 |
Electrical performance | Test Condition | Test Method | Taro Plast S.p.A./TAROMID B 280 G2 X2 |
---|---|---|---|
Volume resistivity | ASTM D257 | 1E+15 ohms·cm | |
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | PLC 2 |
Mechanical properties | Test Condition | Test Method | Taro Plast S.p.A./TAROMID B 280 G2 X2 |
---|---|---|---|
Flexural modulus | ASTMD790 | 4800 MPa | |
elongation | 断裂 | ASTMD638 | 6.0 % |
Tensile modulus | ASTMD638 | 5200 MPa | |
tensile strength | 断裂 | ASTMD638 | 104 MPa |
flammability | Test Condition | Test Method | Taro Plast S.p.A./TAROMID B 280 G2 X2 |
---|---|---|---|
Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 850 °C |
UL flame retardant rating | 1.6mm | UL 94 | V-2 |
Limiting Oxygen Index | ASTM D2863 | 30 % |
physical property | Test Condition | Test Method | Taro Plast S.p.A./TAROMID B 280 G2 X2 |
---|---|---|---|
GranuleHumidity | 内部方法 | <0.100 | |
Shrinkage rate | MD | ASTM D955 | 0.60to0.80 % |
Water absorption rate | 饱和 | ASTM D570 | 7.6 % |
density | ASTMD792 | 1.22 g/cm³ | |
Water absorption rate | 23°C,24hr | ASTMD570 | 1.7 % |
饱和,23°C | ISO 62 | 7.6 % | |
Shrinkage rate | TD | ASTM D955 | 1.2to1.4 % |
Thermal performance | Test Condition | Test Method | Taro Plast S.p.A./TAROMID B 280 G2 X2 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTMD648 | 110 °C |
vicat | -- | ASTMD15254 | 200 °C |
Linear coefficient of thermal expansion | MD:-30到30°C | ASTM D696 | 4.2E-05 cm/cm/°C |
vicat | -- | ASTMD15253 | 204 °C |
ball-indentation hardness | 165°C | VDE0470 | 通过 |
melting temperature | ASTMD211 | 222 °C |