plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA66 Secomid A NERO Poliblend S.p.a.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodPoliblend S.p.a./Secomid A NERO
Ball Pressure Test165°CIEC 60695-10-2通过
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B200 °C
1.8MPa,UnannealedISO 75-2/A70.0 °C
连续使用温度280.0 °C
Melting temperatureDSC260 °C
Vicat softening temperatureISO 306/A120250 °C
mechanical propertiesTest ConditionTest MethodPoliblend S.p.a./Secomid A NERO
Tensile modulusISO 527-23000 MPa
Tensile strainYieldISO 527-24.0 %
BreakISO 527-230 %
tensile strengthYieldISO 527-275.0 MPa
Physical propertiesTest ConditionTest MethodPoliblend S.p.a./Secomid A NERO
densityISO 11831.14 g/cm³
Shrinkage rate1.4to1.8 %
Water absorption rate23°C,24hrISO 621.2 %
impact performanceTest ConditionTest MethodPoliblend S.p.a./Secomid A NERO
Impact strength of cantilever beam gapISO 180/A3.5 kJ/m²
flammabilityTest ConditionTest MethodPoliblend S.p.a./Secomid A NERO
UL flame retardant rating3.2mmUL 94HB
0.8mmUL 94HB
1.6mmUL 94HB