EHMWPE POLYSTONE® MPG R?chling Engineering Plastics SE & Co. KG
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Test Condition | Test Method | R?chling Engineering Plastics SE & Co. KG/POLYSTONE® MPG | |
---|---|---|---|
UL flame retardant rating | 3.0mm | UL 94 | HB |
Charpy Notched Impact Strength | ISO 179 | 无断裂 | |
Shore hardness | 邵氏D | ISO 868 | 65 |
Dissipation Factor | 1MHz | IEC 60250 | 1E-04 |
Continuous use temperature | <130 °C | ||
Volume resistivity | IEC 60093 | >1.0E+14 ohms·cm | |
dielectric constant | IEC 60250 | 2.30 | |
melting temperature | ISO 11357-3 | 135 °C | |
density | ISO 1183 | 0.960 g/cm³ | |
Heat distortion temperature | VicatB,HDT | ISO 306 | 79 °C |
Linear coefficient of thermal expansion | MD | DIN 53752 | 1.5E-4到2.3E-4 cm/cm/°C |
tensile strength | 屈服 | ISO 527-2 | 22.0 MPa |
Surface Resistivity | IEC 60093 | >1.0E+12 ohms | |
Tensile modulus | ISO 527-2 | 800 MPa | |
thermal conductivity | DIN 52612 | 0.40 W/m/K | |
Tensile strain | 断裂 | ISO 527-2 | >200 % |
WearResistance-Sand-slurrymethod | 82.0 | ||
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | PLC 0 | |
specific heat | DIN 52612 | 1900 J/kg/°C | |
dielectric strength | IEC 60243-1 | 45 kV/mm | |
UL flame retardant rating | 6.0mm | UL 94 | HB |
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | <0.010 % |