ETPU ISOPLAST™ 302EZ TPU Lubrizol Advanced Materials, Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodLubrizol Advanced Materials, Inc./ISOPLAST™ 302EZ TPU
Impact strength of cantilever beam gap23°C,3.20mmASTM D256110 J/m
Dart impact23°C,TotalEnergyASTM D376368.0 J
Impact strength of cantilever beam gap-40°C,3.20mmASTM D25659 J/m
hardnessTest ConditionTest MethodLubrizol Advanced Materials, Inc./ISOPLAST™ 302EZ TPU
Rockwell hardnessM级ASTM D78592
R级ASTM D785124
Mechanical propertiesTest ConditionTest MethodLubrizol Advanced Materials, Inc./ISOPLAST™ 302EZ TPU
elongation断裂ASTM D63830 %
屈服ASTM D6389.0 %
Tensile modulusASTM D6381900 MPa
tensile strength 断裂ASTM D63869.0 MPa
Flexural modulusASTM D7902300 MPa
tensile strength 屈服ASTM D63883.0 MPa
bending strengthASTM D79097.0 MPa
optical performance Test ConditionTest MethodLubrizol Advanced Materials, Inc./ISOPLAST™ 302EZ TPU
transmissivityASTM D100388.0 %
Yellowness IndexASTM D192540 YI
physical property Test ConditionTest MethodLubrizol Advanced Materials, Inc./ISOPLAST™ 302EZ TPU
Shrinkage rateMDASTM D9550.40to0.60 %
densityASTM D7921.20 g/cm³
Thermal performanceTest ConditionTest MethodLubrizol Advanced Materials, Inc./ISOPLAST™ 302EZ TPU
Heat distortion temperature1.8MPa,未退火,HDTASTM D648116 °C
vicatASTM D1525147 °C
Heat distortion temperature0.45MPa,未退火,HDTASTM D648132 °C
1.8MPa,退火,HDTASTM D648138 °C
Linear coefficient of thermal expansionMDASTM D6965.8E-05 cm/cm/°C
Heat distortion temperature0.45MPa,退火,HDTASTM D648143 °C