Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 B3 GF 30 AKRO-PLASTIC GERMANY
AKROMID®
Engineering accessories,Automotive sector,engineering application ,engineering application
high strength,High rigidity,Glass fiber reinforced,enhance,Filler: Glass fiber reinf,30% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
Ball Pressure Test | H961/30 | ISO 2039-1 | 230 Mpa |
Supplementary Information | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
ReinforcementContent | ISO 1172 | 30 % |
thermal performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
Hot deformation temperature | 8.0MPa,Unannealed | ISO 75-2/C | 150 °C |
0.45MPa,Unannealed | ISO 75-2/B | 220 °C | |
1.8MPa,Unannealed | ISO 75-2/A | 210 °C | |
Linear coefficient of thermal expansion | TD:23to80°C | ISO 11359-2 | 9.5E-05 cm/cm/°C |
MD:23to80°C | ISO 11359-2 | 1.6E-05 cm/cm/°C | |
Melting temperature | DIN EN11357-1 | 220 °C | |
TemperatureIndex | 50%LossofTensileStrength,20000hr | IEC 216 | 130to150 °C |
50%LossofTensileStrength,5000hr | IEC 216 | 160to175 °C |
mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
Bending modulus | ISO 178 | 8500 Mpa | |
bending strength | ISO 178 | 270 Mpa | |
Tensile modulus | ISO 527-2/1 | 10300 Mpa | |
Tensile strain | Break | ISO 527-2/5 | 3.0 % |
tensile strength | Break | ISO 527-2/5 | 185 Mpa |
Electrical performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
Compared to the anti leakage trace index | SolutionA | IEC 60112 | V |
Surface resistivity | IEC 60093 | 1E+12 ohms | |
Volume resistivity | IEC 60093 | 1E+13 ohms·cm |
Physical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
Hygroscopicity | 70°C,62%RH | ISO 1110 | 2.1to2.3 % |
Shrinkage rate | MD | ISO 294-4 | 0.10 % |
TD | ISO 294-4 | 0.80 % | |
Spiral flow length | Internal Method | 66.0 CM | |
Water absorption rate | Saturation,23°C | ISO 62 | 6.3to6.9 % |
impact performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 85 kJ/m² |
23°C | ISO 179/1eU | 95 kJ/m² |
flammability | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 30 |
---|---|---|---|
Burning rate | 1.00mm | FMVSS302 | <100 mm/min |
Burning wire flammability index | 1.6mm | IEC 60695-2-12 | 650 °C |
UL flame retardant rating | 1.6mm | UL 94 | HB |