PC/ABS NF004 SABIC INNOVATIVE NANSHA
LNP™ THERMOCOMP™
Plastic bag,Gears,Casters
High mobility,High impact resistance,Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/NF004 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 135 °C |
0.45MPa,Unannealed,64.0mmSpan | ISO 75-2/Bf | 140 °C | |
1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 134 °C | |
0.45MPa,Unannealed,3.20mm | ASTM D648 | 139 °C | |
Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7.7E-05 cm/cm/°C |
TD:-40to40°C | ISO 11359-2 | 3.2E-05 cm/cm/°C | |
TD:-40to40°C | ASTME831 | 3.2E-05 cm/cm/°C | |
MD:-40to40°C | ISO 11359-2 | 7.7E-05 cm/cm/°C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/NF004 |
---|---|---|---|
Bending modulus | ISO 178 | 6000 Mpa | |
ASTM D790 | 6210 Mpa | ||
bending strength | ASTM D790 | 138 Mpa | |
ISO 178 | 143 Mpa | ||
elongation | Break | ASTM D638 | 2.5 % |
Tensile modulus | ISO 527-2/1 | 6480 Mpa | |
ASTM D638 | 6890 Mpa | ||
Tensile strain | Break | ISO 527-2 | 2.6 % |
tensile strength | Break | ASTM D638 | 97.2 Mpa |
Break | ISO 527-2 | 95.0 Mpa |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/NF004 |
---|---|---|---|
Shrinkage rate | TD:24hr | ASTM D955 | 0.60 % |
TD:24hr | ISO 294-4 | 0.58 % | |
MD:24hr | ASTM D955 | 0.40 % | |
MD:24hr | ISO 294-4 | 0.41 % | |
Water absorption rate | 24hr,50%RH | ASTM D570 | 0.10 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/NF004 |
---|---|---|---|
Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 18.2 J |
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 11 kJ/m² |
Multi axis Instrumented Impact Energy | ISO 6603-2 | 5.20 J | |
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 37 kJ/m² |