Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC 503RS-9T7D006L SABIC INNOVATIVE NETHERLANDS
LEXAN™
fibre
High impact resistance、High rigidity、Glass fiber reinforced、enhance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | SABIC INNOVATIVE NETHERLANDS/503RS-9T7D006L |
---|---|---|---|
Simply supported beam without notch impact strength 5 | -30°C | ISO179/1eU | 无断裂 |
Impact strength of simply supported beam gap 4 | 23°C | ISO179/1eA | 9.0 kJ/m² |
Simply supported beam without notch impact strength 5 | 23°C | ISO179/1eU | 无断裂 |
-30°C | ISO180/1U | 100 kJ/m² | |
23°C | ISO180/1U | 无断裂 | |
Suspended wall beam notch impact strength 6 | -30°C | ISO180/1A | 8.0 kJ/m² |
23°C | ISO180/1A | 9.0 kJ/m² | |
Impact strength of simply supported beam gap 4 | -30°C | ISO179/1eA | 8.0 kJ/m² |
hardness | Test Condition | Test Method | SABIC INNOVATIVE NETHERLANDS/503RS-9T7D006L |
---|---|---|---|
H358/30 | ISO2039-1 | 115 Mpa |
Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE NETHERLANDS/503RS-9T7D006L |
---|---|---|---|
Surface Resistivity | IEC60093 | >1.0E+15 ohms | |
50Hz | IEC60250 | 2.90 | |
dielectric strength | 3.20mm,在油中 | IEC60243-1 | 16 KV/mm |
Volume resistivity | IEC60093 | >1.0E+15 ohms·cm | |
Dissipation Factor | 60Hz | IEC60250 | 1E-03 |
50Hz | IEC60250 | 1E-03 | |
1MHz | IEC60250 | 0.010 | |
60Hz | IEC60250 | 2.90 | |
1MHz | IEC60250 | 2.80 |
Mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE NETHERLANDS/503RS-9T7D006L |
---|---|---|---|
Tensile stress | 断裂 | ISO527-2/5 | 65.0 Mpa |
屈服 | ISO527-2/5 | 70.0 Mpa | |
Tensile modulus | ISO527-2/1 | 3900 Mpa | |
Tensile strain | 断裂 | ISO527-2/5 | 4.0 % |
屈服 | ISO527-2/5 | 3.0 % | |
Bending modulus 2 | ISO178 | 4000 Mpa | |
Bending stress 3 | ISO178 | 120 Mpa |
flammability | Test Condition | Test Method | SABIC INNOVATIVE NETHERLANDS/503RS-9T7D006L |
---|---|---|---|
UL flame retardant rating | 1.50mm,TestingbySABIC | UL94 | V-0 |
Burning wire flammability index | 1.00mm | IEC60695-2-12 | 960 °C |
Limiting Oxygen Index | ISO4589-2 | 36 % |
physical property | Test Condition | Test Method | SABIC INNOVATIVE NETHERLANDS/503RS-9T7D006L |
---|---|---|---|
Water absorption rate | 平衡,23°C,50%RH | ISO62 | 0.13 % |
饱和,23°C | ISO62 | 0.31 % | |
Melt volume flow rate | 300°C/1.2kg | ISO1133 | 8.00 cm3/10min |
Shrinkage rate | MD1 | 内部方法 | 0.20到0.60 % |
Thermal performance | Test Condition | Test Method | SABIC INNOVATIVE NETHERLANDS/503RS-9T7D006L |
---|---|---|---|
1.8MPa, Unanealed, 100mm span | ISO75-2/Ae | 137 °C | |
BallPressure Test | 125°C | IEC60695-10-2 | Pass |
MD:23到80°C | ISO11359-2 | 4E-05 cm/cm/°C | |
0.45MPa, Unanealed, 100mm span | ISO75-2/Be | 142 °C | |
thermal conductivity | ISO8302 | 0.21 W/m/K |
Contact Us
Get App
Top