LDPE 352E SADARA SAUDI
DOW™
Food packaging、Flexible packaging
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | SADARA SAUDI/352E |
---|---|---|---|
melt mass-flow rate | 190℃/2.16kg | ISO 1133 | 2 g/10min |
film thickness | 50 um | ||
density | ASTM D-792 | 0.925 g/m3 |
Mechanical properties | Test Condition | Test Method | SADARA SAUDI/352E |
---|---|---|---|
Secant modulus | 50um,TD | ASTM D-882 | 210 Mpa |
elongation at break | 50um,MD | ASTM D-882 | 450 % |
Secant modulus | 50um,MD | ASTM D-882 | 190 Mpa |
tensile strength | 50um,屈服,TD | ASTM D-882 | 11 Mpa |
Elmendorf tear strength | 50um,MD | ASTM D-1922 | 450 g |
coefficient of friction | vs. Itself - Dynamic | ASTM D-1894 | 0.15-2 |
elongation at break | 50um,TD | ASTM D-882 | 650 % |
tensile strength | 50um,MD,断裂 | ASTM D-882 | 22 Mpa |
50um,TD,断裂 | ASTM D-882 | 20 Mpa | |
Dart impact | 50um | ASTM D-1709A | 110 g |
tensile strength | 50um,屈服,MD | ASTM D-882 | 10 Mpa |
Elmendorf tear strength | 50um,TD | ASTM D-1922 | 350 g |
optical performance | Test Condition | Test Method | SADARA SAUDI/352E |
---|---|---|---|
Haze ratio | 50um | ASTM D-1003 | 8 % |
gloss | 20°,50um | ASTM D-2457 | 60 |
processability | Test Condition | Test Method | SADARA SAUDI/352E |
---|---|---|---|
Melt Temperature | 160-175 °C |