Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS Pyramid™ SC100 Polymics, Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | Polymics, Ltd./Pyramid™ SC100 |
---|---|---|---|
process temperature | 310to343 °C | ||
Thermal decomposition temperature | ASTM D648 | 371 °C |
Mechanical properties | Test Condition | Test Method | Polymics, Ltd./Pyramid™ SC100 |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 1.0 % |
tensile strength | ASTM D638 | 203 MPa | |
Tensile modulus | ASTM D638 | 33000 MPa |
physical property | Test Condition | Test Method | Polymics, Ltd./Pyramid™ SC100 |
---|---|---|---|
density | ASTM D792 | 1.50 g/cm³ |
Thermal performance | Test Condition | Test Method | Polymics, Ltd./Pyramid™ SC100 |
---|---|---|---|
melting temperature | ASTM D3418 | 280 °C |
Contact Us
Get App
Top