Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

mechanical propertiesTest ConditionTest MethodKURARAY JAPAN/HR1000L
Rockwell hardnessASTM D-785105 M Scale
ASTM D785105
Impact strength of cantilever beam gapASTM D-2561.6 kg.cm/cm
bending strengthASTM D-7901240 kg/cm
Bending modulusASTM D790/ISO 17835000 kg/cm²(MPa)[Lb/in²]
ASTM D-79035000 kg/cm
tensile strengthASTM D-638770 %
Basic PerformanceTest ConditionTest MethodKURARAY JAPAN/HR1000L
Water absorption rateASTM D-5700.3 %
melt mass-flow rate230℃/3.8kgsASTM D-12382.1 g/10min
thermal performanceTest ConditionTest MethodKURARAY JAPAN/HR1000L
Hot deformation temperatureHDTASTM D648/ISO 7597 ℃(℉)
CombustibilityUL 94HB CLASS
Hot deformation temperature无AnnealedASTM D-64897 °C
Vicat softening temperatureASTM D-1525118 °C
ASTM D1525/ISO R306118 ℃(℉)
Hot deformation temperature有AnnealedASTM D-648106 °C
Combustibility (rate)UL 94HB
Physical propertiesTest ConditionTest MethodKURARAY JAPAN/HR1000L
Transmittance rateASTM D-100393 %
Shrinkage rateASTM D9550.002-0.006 %
ASTM D-9550.002-0.006 %
Refractive indexASTM D-5421.49
densityASTM D792/ISO 11831.19
otherTest ConditionTest MethodKURARAY JAPAN/HR1000L
characteristic耐热性、挤出
Other performanceTest ConditionTest MethodKURARAY JAPAN/HR1000L
BezASTM D-10030.3 %