Thermal Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Deflection Temperature Under Load? | 1.8 MPa, 未退火, 3.20 mm | ASTM D648 | 128 °C |
Injection | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Suggested Max Moisture | 0.020 % | ||
Middle Temperature | 305 到 315 °C | ||
Processing (Melt) Temp | 300 到 315 °C | ||
Drying Time | 4.0 hr | ||
Rear Temperature | 295 到 305 °C | ||
Drying Temperature | 120 °C | ||
Front Temperature | 310 到 320 °C | ||
Back Pressure | 0.200 到 0.300 Mpa | ||
Mold Temperature | 80 到 110 °C | ||
Screw Speed | 30 到 60 rpm |
Physical | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Modeling Shrinkage | 流动 : 24小时 | ASTM D955 | 0.70 到 0.90 % |
横向流动 : 24小时 | 0.70 到 0.90 % |
Mechanical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Flexural Strength | ASTM D790 | 81.0 Mpa | |
Specific Wear Rate | ASTM D3702 | 2.0E+7 10^-8 mm³/N·m | |
Flexural Modulus | ASTM D790 | 2270 Mpa | |
Coefficient of Friction | Dynamic | ASTM D3702 | 0.28 |
Tensile Strength | 断裂 | ASTM D638 | 53.0 Mpa |
Tensile Elongation | 53 % | ||
Coefficient of Friction | Static | ASTM D3702 | 0.17 |
Impact Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Unnotched Izod Impact Strength | 23°C | ASTM D4812 | 无断裂 |