Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PUR-MDI Andur M-80 AS USA Anderson Development
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermosetting | Test Condition | Test Method | USA Anderson Development/Andur M-80 AS |
|---|---|---|---|
| storage stability | 2.5 min | ||
| stripping time | 15 min | ||
| Thermosetting mixed viscosity | 21°C | ASTM D2393 | 770 cP |
| Physical properties | Test Condition | Test Method | USA Anderson Development/Andur M-80 AS |
|---|---|---|---|
| density | ASTM D792 | 1.22 g/cm³ |