Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA9T NT363 OTSUKAC JAPAN
POTICON
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | OTSUKAC JAPAN/NT363 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ASTM D785 | 95 |
| thermal performance | Test Condition | Test Method | OTSUKAC JAPAN/NT363 |
|---|---|---|---|
| Heat Distortion | ASTM D648 | 200 °C | |
| Linear coefficient of thermal expansion | Flow | ASTM D696 | 2.3E-5 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | OTSUKAC JAPAN/NT363 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 11200 Mpa | |
| bending strength | ASTM D790 | 238 Mpa | |
| elongation | Break | ASTM D638 | 3.1 % |
| Friction coefficient | 与钢 - 动态 | 0.14 | |
| tensile strength | ASTM D638 | 150 Mpa | |
| Wear amount | of counterpart 4 | 0.00 10^-3 mm³/N·km | |
| --3 | 1.80 10^-3 mm³/N·km |
| Physical properties | Test Condition | Test Method | OTSUKAC JAPAN/NT363 |
|---|---|---|---|
| Shrinkage rate | Across FlowFlow | 1.0 % | |
| Flow | 0.50 % | ||
| Water absorption rate | Equilibrium | ASTM D570 | 0.20 % |
| flammability | Test Condition | Test Method | OTSUKAC JAPAN/NT363 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |
| injection | Test Condition | Test Method | OTSUKAC JAPAN/NT363 |
|---|---|---|---|
| Injection pressure | 40.0 to 60.0 Mpa | ||
| Mold temperature | 120 to 150 °C | ||
| Processing (melt) temperature | 260 to 280 °C |