Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP STERLENE™ KB010-A4001 R&P (Pte.) Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodR&P (Pte.) Ltd./STERLENE™ KB010-A4001
Impact strength of cantilever beam gap23°C,完全断裂ISO 180/A5.0 kJ/m²
Mechanical propertiesTest ConditionTest MethodR&P (Pte.) Ltd./STERLENE™ KB010-A4001
tensile strength 屈服,23°CISO 527-2/5023.0 MPa
Flexural modulus23°CISO 1781900 MPa
Tensile strain屈服,23°CISO 527-2/504.0 %
断裂,23°CISO 527-2/5023 %
bending strength23°CISO 17836.0 MPa
physical property Test ConditionTest MethodR&P (Pte.) Ltd./STERLENE™ KB010-A4001
Water absorption rate23°C,24hr内部方法0.041 %
densityISO 11831.00 g/cm³
ash content600°C内部方法19 %
melt mass-flow rate230°C/2.16kgISO 113332 g/10min
Thermal performanceTest ConditionTest MethodR&P (Pte.) Ltd./STERLENE™ KB010-A4001
Heat distortion temperature1.8MPa,未退火,HDTISO 75-2/Af59.0 °C

Contact Us

Get App

Top