Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| Physical properties | Test Condition | Test Method | DUPONT USA/73G30T NC010 |
|---|---|---|---|
| ThermalConductivityofMelt | 0.23 W/m/K | ||
| Top out temperature | 210 °C | ||
| density | ISO 1183 | 1.35 g/cm³ | |
| MediumDensity | 1.31 g/cm³ | ||
| Shrinkage rate | MD | ISO 294-4 | 0.20 % |
| SpecificHeatCapacity of Melt | 2200 J/kg/°C | ||
| Shrinkage rate | TD | ISO 294-4 | 1.0 % |
| Water absorption rate | Saturation,23°C,2.00mm | ISO 62 | 6.2 % |
| Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 1.8 % | |
| flammability | Test Condition | Test Method | DUPONT USA/73G30T NC010 |
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | HB |
| Burning rate | 1.00mm | ISO 3795 | <100 mm/min |
| FMVSS flammability | FMVSS302 | B | |
| impact performance | Test Condition | Test Method | DUPONT USA/73G30T NC010 |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 14 kJ/m² |
| -30°C | ISO 179/1eA | 10 kJ/m² | |
| thermal performance | Test Condition | Test Method | DUPONT USA/73G30T NC010 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 210 °C |
| Linear coefficient of thermal expansion | MD2 | ISO 11359-2 | 3E-05 cm/cm/°C |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 206 °C |
| Linear coefficient of thermal expansion | TD2 | ISO 11359-2 | 1.2E-04 cm/cm/°C |
| Melting temperature | ISO 11357-3 | 220 °C | |
| Vicat softening temperature | ISO 306/B50 | 210 °C | |
| mechanical properties | Test Condition | Test Method | DUPONT USA/73G30T NC010 |
| Tensile strain | Break | ISO 527-2 | 3.3 % |
| tensile strength | Break | ISO 527-2 | 160 Mpa |
| Tensile modulus | ISO 527-2 | 9500 Mpa |