| mechanical properties | Test Condition | Test Method | SK KOREA/S385A |
|---|---|---|---|
| elongation | Break | 780 % | |
| tear strength | ASTM D-624 | 93.2 kN/m | |
| tensile strength | Yield | 34.3 MPa | |
| 100%Strain | ASTM D-412 | 5.39 Mpa | |
| Wear amount | ISO 4649 | 35 mm³ | |
| Permanent compression deformation | 23℃,22.0hr | ASTM D-395 | 15 % |
| tensile strength | 300%Strain | 9.81 MPa | |
| Physical properties | Test Condition | Test Method | SK KOREA/S385A |
| Shrinkage rate | MD | ASTM D-955 | 2.6 % |
| Shore hardness | ShoreA | ASTM D-2240 | 85 |
| thermal performance | Test Condition | Test Method | SK KOREA/S385A |
| Vicat softening temperature | ASTM D-1525 | 62 °C |