Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EHMWPE Paxon™ BA50-100 ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ExxonMobil/Paxon™ BA50-100 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ASTM D1822 | 252 kJ/m² |
Mechanical properties | Test Condition | Test Method | ExxonMobil/Paxon™ BA50-100 |
---|---|---|---|
Flexural modulus | ASTM D790 | 1240 MPa | |
tensile strength | 屈服 | ASTM D638 | 26.0 MPa |
physical property | Test Condition | Test Method | ExxonMobil/Paxon™ BA50-100 |
---|---|---|---|
melt mass-flow rate | 190°C/21.6kg | ASTM D1238 | 10 g/10min |
Environmental stress cracking resistance | 100%Igepal | ASTM D1693 | >800 hr |
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | <0.10 g/10min |
density | ASTM D4883 | 0.949 g/cm³ |
Thermal performance | Test Condition | Test Method | ExxonMobil/Paxon™ BA50-100 |
---|---|---|---|
vicat | ASTM D1525 | 120 °C | |
brittle temperature | ASTM D746 | <-76.0 °C |
Contact Us
Get App
Top