Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
LCP S471-BK010P JAPAN POLYPLASTIC
LAPEROS® 
Electrical applications、Home appliance components
enhance、Glass fiber reinforced
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodJAPAN POLYPLASTIC/S471-BK010P
Impact strength of simply supported beam without notch23°CISO 179/1eU10 kJ/m²
Mechanical propertiesTest ConditionTest MethodJAPAN POLYPLASTIC/S471-BK010P
bending strength23°CISO 178185 Mpa
Flexural modulus23°CISO 17812000 Mpa
tensile strength 断裂ISO 527-2/1A/5120 Mpa
Tensile strain断裂ISO 527-2/1A/51.4 %
Fracture bending strainISO 1782.0 %
Tensile modulusISO 527-2/1A12000 Mpa
Electrical performanceTest ConditionTest MethodJAPAN POLYPLASTIC/S471-BK010P
Dissipation Factor1 MHzIEC 602507.0E-3
Volume resistivityIEC 600931.0E+16 ohms·cm
relative permittivity1 MHzIEC 602504.00
Surface ResistivityIEC 600931.0E+11 ohms
Compared to the Leakage Tracking Index (CTI)IEC 60112 V
flammabilityTest ConditionTest MethodJAPAN POLYPLASTIC/S471-BK010P
UL flame retardant ratingUL 94V-0
physical property Test ConditionTest MethodJAPAN POLYPLASTIC/S471-BK010P
Shrinkage rate流量ISO 294-40.20 %
横向流量ISO 294-40.50 %
Thermal performanceTest ConditionTest MethodJAPAN POLYPLASTIC/S471-BK010P
melting temperatureISO 11357-3350 °C
Heat distortion temperature1.8 MPa, 未退火,HDTISO 75-2/A315 °C
8.0 MPa, 未退火,HDTISO 75-2/C271 °C
Linear coefficient of thermal expansion流动ISO 11359-28.0E-6 cm/cm/°C
横向ISO 11359-21.7E-5 cm/cm/°C
injectionTest ConditionTest MethodJAPAN POLYPLASTIC/S471-BK010P
drying time6.0 hr
Temperature in the middle of the barrel340 to 360 °C
Temperature at the rear of the barrel330 to 350 °C
Processing (melt) temperature360 to 375 °C
Hopper temperature20 to 40 °C
drying temperature150 to 170 °C
Temperature at the front of the material cylinder345 to 365 °C
Back pressure< 3.00 Mpa
Temperature80 to 120 °C
injection speed中等
Spray nozzle temperature355 to 370 °C

Contact Us