Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPEE HTR8685 BK022A DUPONT USA
Hytrel®
Automotive Applications、Cable、Blow molding applications
High temperature resistan、Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 44 |
邵氏D,15秒 | ISO 868 | 41 |
Mechanical properties | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Tensile modulus | ISO 527-2 | 100 Mpa | |
Nominal tensile fracture strain | ISO 527-2 | 350 % | |
tensile strength | 10%应变 | ISO 527-2 | 8.40 Mpa |
Tensile strain | 断裂 | ISO 527-2 | >300 % |
Flexural modulus | ISO 178 | 100 Mpa | |
tensile strength | 断裂 | ISO 527-2 | 30.0 Mpa |
50%应变 | ISO 527-2 | 14.0 Mpa |
flammability | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
FMVSS flammability | FMVSS302 | B | |
burning rate | 1.00mm | ISO 3795 | <100 mm/min |
physical property | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 1.6 % |
MD | ISO 294-4 | 1.7 % |
elastomer | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
tear strength | 流量 | ISO 34-1 | 110 kN/m |
横向流量 | ISO 34-1 | 110 kN/m |
Thermal performance | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
melting temperature | ISO 11357-3 | 206 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 2.1E-04 cm/cm/°C |
TD | ISO 11359-2 | 2E-04 cm/cm/°C |