PC DL-4020FR BK SABIC INNOVATIVE US
LNP™ LUBRICOMP™
Plastic bag,Electrical appliances,Electronic and Electrical Applications
Easy to form,Easy to demould
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Hot deformation temperature | 1.8 MPa, 未退火, 3.20 mm | ASTM D648 | 128 °C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Bending modulus | ASTM D790 | 2270 Mpa | |
bending strength | ASTM D790 | 81.0 Mpa | |
elongation | 断裂 | ASTM D638 | 53 % |
Friction coefficient | Static | ASTM D3702 | 0.17 |
Dynamic | ASTM D3702 | 0.28 | |
tensile strength | 断裂 | ASTM D638 | 53.0 Mpa |
Wear factor | ASTM D3702 | 2.0E+7 10^-8 mm³/N·m |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Shrinkage rate | 横向流动 : 24小时 | ASTM D955 | 0.70 - 0.90 % |
流动 : 24小时 | ASTM D955 | 0.70 - 0.90 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Suspended wall beam without notch impact strength | 23°C | ASTM D4812 | 无断裂 |
injection | Test Condition | Test Method | SABIC INNOVATIVE US/DL-4020FR BK |
---|---|---|---|
Back pressure | 0.200 to 0.300 Mpa | ||
drying temperature | 120 °C | ||
drying time | 4.0 hr | ||
Mold temperature | 80 to 110 °C | ||
Processing (melt) temperature | 300 to 315 °C | ||
Screw speed | 30 to 60 rpm | ||
Suggested maximum moisture content | 0.020 % | ||
Temperature at the front of the material cylinder | 310 to 320 °C | ||
Temperature at the rear of the barrel | 295 to 305 °C | ||