Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PET 130FR NC BASF GERMANY
Petra®
--
30% glass fiber reinforce、Chemical resistance、Good thermal stability an
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | BASF GERMANY/130FR NC |
---|---|---|---|
Limiting Oxygen Index | ISO 4589-1 | 36 % |
Mechanical properties | Test Condition | Test Method | BASF GERMANY/130FR NC |
---|---|---|---|
Impact strength of cantilever beam gap | 73℉ | ASTM D256 | 1.69 ft·lb/in |
Tensile modulus | ISO 527-1 | 1.61E+06 psi | |
elongation | 断裂 | ASTM D638 | 2.0 % |
tensile strength | 断裂 | ASTM D638 | 18900 psi |
bending strength | 248℉ | ASTM D790 | 12300 psi |
Breaking stress | ISO 527-1 | 19000 psi | |
Flexural modulus | -40℉ | ASTM D790 | 1.8E+06 psi |
bending strength | 73℉ | ASTM D790 | 30500 psi |
Flexural modulus | 248℉ | ASTM D790 | 431000 psi |
bending strength | -40℉ | ASTM D790 | 39900 psi |
Flexural modulus | 73℉ | ASTM D 790 | 1.41E+06 psi |
fracture strain | ISO 527-1 | 2.0 % |
Electrical performance | Test Condition | Test Method | BASF GERMANY/130FR NC |
---|---|---|---|
dielectric constant | 100HZ | IEC 60250 | 3.80 |
1MHz | IEC 60250 | 3.60 | |
Volume resistivity | IEC 60093 | >3.9E+12 ohm·in |
physical property | Test Condition | Test Method | BASF GERMANY/130FR NC |
---|---|---|---|
Rockwell hardness | ASTM D785 | 118 |
Thermal performance | Test Condition | Test Method | BASF GERMANY/130FR NC |
---|---|---|---|
Heat distortion temperature | 0.45MPa,HDT | ISO 75-1 | 464 ℉ |
melting temperature | 473 ℉ | ||
Heat distortion temperature | 1.80MPa,HDT | ISO 75-1 | 410 ℉ |
UL flame retardant rating | UL 94 | V-0 |
Contact Us
Get App
Top