Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Biodeg Polymers silk twoBEars GbR
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | twoBEars GbR/ silk |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 6.8 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 58 kJ/m² |
-15°C | ISO 179/1eU | 37 kJ/m² |
hardness | Test Condition | Test Method | twoBEars GbR/ silk |
---|---|---|---|
ball-indentation hardness | ISO 2039-1 | 105 MPa | |
Shore hardness | 邵氏D | DIN 53505 | 75 |
Mechanical properties | Test Condition | Test Method | twoBEars GbR/ silk |
---|---|---|---|
tensile strength | -- | ISO 527-2 | 51.0 MPa |
Tensile modulus | ISO 527-2 | 2700 MPa | |
tensile strength | 断裂 | ISO 527-2 | 22.8 MPa |
Tensile strain | 断裂 | ISO 527-2 | 12 % |
屈服 | ISO 527-2 | 2.5 % | |
Flexural modulus | ISO 178 | 1810 MPa | |
bending strength | ISO 178 | 70.0 MPa |
physical property | Test Condition | Test Method | twoBEars GbR/ silk |
---|---|---|---|
Melt volume flow rate | 190°C/2.16kg | ISO 1133 | 3.00 cm³/10min |
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | 0.50 % |
density | ISO 1183 | 1.25 g/cm³ |
Thermal performance | Test Condition | Test Method | twoBEars GbR/ silk |
---|---|---|---|
vicat | ISO 306/A50 | 58.4 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 50.4 °C |
thermal conductivity | 10°C | DIN 52612 | 0.17 W/m/K |
melting temperature | ISO 3146 | 153 °C |