Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PUR-Ether//TDI 442 USA Anderson Development
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodUSA Anderson Development/ 442
Shore hardness邵氏DASTM D224061
邵氏AASTM D224080
Mechanical propertiesTest ConditionTest MethodUSA Anderson Development/ 442
compressive strength10%应变ASTM D6951.10 MPa
25%应变ASTM D6953.17 MPa
5%应变ASTM D6950.421 MPa
15%应变ASTM D6951.94 MPa
thermosettingTest ConditionTest MethodUSA Anderson Development/ 442
Post curing time100°C16 hr
STORAGE STABILITY10to12 min
stripping time100°C15 min
Post curing time96°C16 hr
stripping time30 min
elastomerTest ConditionTest MethodUSA Anderson Development/ 442
elongation断裂ASTM D412550 %
tensile strength 屈服ASTM D41231.7 MPa
Shore hardnessASTM D263220 %
compression setASTM D395B34 %
tensile strength 100%应变ASTM D4124.69 MPa
300%应变ASTM D4128.27 MPa
physical property Test ConditionTest MethodUSA Anderson Development/ 442
densityASTM D15051.12 g/cm³
Shrinkage rateMDASTM D9551.2 %