| elastomer | Test Condition | Test Method | DSM HOLAND/3170B |
|---|---|---|---|
| tensile strength | Flow:Break | ISO 37 | 6.70 Mpa |
| elongation | Flow:Break | ISO 37 | 300 % |
| Flow:Break | ASTM D412 | 300 % | |
| tensile strength | Flow:Break | ASTM D412 | 6.70 Mpa |
| tear strength | 横向Flow | ASTM D624 | 42.0 kN/m |
| tensile strength | 横向Flow:100%Strain | ISO 37 | 3.30 Mpa |
| Permanent compression deformation | 70°C,22hr | ASTM D395 | 43 % |
| 23°C,22hr | ISO 815 | 25 % | |
| tensile strength | Break | ISO 37 | 7.70 Mpa |
| Permanent compression deformation | 70°C,22hr | ISO 815 | 43 % |
| 125°C,70hr | ISO 815 | 63 % | |
| tensile strength | Flow:100%Strain | ASTM D412 | 5.10 Mpa |
| tear strength | 横向Flow | ISO 34-1 | 42 kN/m |
| elongation | Break | ISO 37 | 670 % |
| tensile strength | Flow:100%Strain | ISO 37 | 5.10 Mpa |
| 横向Flow:100%Strain | ASTM D412 | 3.30 Mpa | |
| Permanent compression deformation | 23°C,22hr | ASTM D395 | 25 % |
| elongation | Break | ASTM D412 | 670 % |
| Permanent compression deformation | 125°C,70hr | ASTM D395 | 63 % |
| tensile strength | Break | ASTM D412 | 7.72 Mpa |
| Supplementary Information | Test Condition | Test Method | DSM HOLAND/3170B |
| ApparentShearViscosity-Capillary,@206/s | 200°C | ISO 11443 | 290 Pa·s |
| 200°C | ASTM D3835 | 290 Pa·s | |
| aging | Test Condition | Test Method | DSM HOLAND/3170B |
| Change rate of ultimate elongation in air | 150°C,168hr,Across Flow | ASTM D573 | -14 % |
| Change rate of tensile strength in air | 150°C,168hr,Across Flow | ASTM D573 | -4.0 % |
| 135°C,1000hr,Across Flow | ASTM D573 | -8.0 % | |
| 100%Strain,150°C,168hr,Across Flow | ASTM D573 | 5.0 % | |
| Change rate of hardness (Shore) in the air | ShoreA,150°C,168hr | ISO 188 | 3.0 |
| Tensile stress change rate | 150°C,168hr,Break | ISO 188 | -14 % |
| Change rate of tensile strength in air | 150°C,168hr,Across Flow | ISO 188 | -4.0 % |
| Volume change | 125°C,70hr,在IRM903油中 | ASTM D471 | 120 % |
| Change rate of tensile strength in air | 135°C,1000hr,Across Flow | ISO 188 | -8.0 % |
| Change rate of hardness (Shore) in the air | ShoreA,135°C,1000hr | ASTM D573 | -1.0 |
| Change rate of tensile strength in air | 100%Strain150°C,168hr,Across Flow | ISO 188 | 5.0 % |
| Change rate of hardness (Shore) in the air | ShoreA,135°C,1000hr | ISO 188 | -1.0 |
| Volume change | 125°C,70hr,在IRM903油中 | ISO 1817 | 120 % |
| Change rate of tensile strength in air | 100%Strain135°C,1000hr,Across Flow | ISO 188 | 10 % |
| 100%Strain,135°C,1000hr,Across Flow | ASTM D573 | 10 % | |
| Change rate of hardness (Shore) in the air | ShoreA,150°C,168hr | ASTM D573 | 3.0 |
| Change rate of ultimate elongation in air | 135°C,1000hr,Across Flow | ASTM D573 | -13 % |
| Tensile stress change rate | 135°C,1000hr,Break | ISO 188 | -13 % |
| hardness | Test Condition | Test Method | DSM HOLAND/3170B |
| Shore hardness | ShoreA,5Sec,Injection | ASTM D2240 | 75 |
| ShoreA,5Sec,挤塑 | ASTM D2240 | 71 | |
| ShoreA,5Sec,挤塑 | ISO 868 | 71 | |
| ShoreA,5Sec,Injection | ISO 868 | 75 | |
| thermal performance | Test Condition | Test Method | DSM HOLAND/3170B |
| RTI Elec | UL 746 | 50.0 °C | |
| RTI Imp | UL 746 | 50.0 °C | |
| RTI Str | UL 746 | 50.0 °C | |
| flammability | Test Condition | Test Method | DSM HOLAND/3170B |
| UL flame retardant rating | 1.5mm | UL 94 | HB |