Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Plastomer, Ethylene-based IDI SMC E-205 IDI Composites International
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | IDI Composites International/IDI SMC E-205 |
---|---|---|---|
Impact strength of cantilever beam gap | ASTM D256 | 750 J/m |
hardness | Test Condition | Test Method | IDI Composites International/IDI SMC E-205 |
---|---|---|---|
Barcol Hardness | ASTM D2583 | 30to50 |
Electrical performance | Test Condition | Test Method | IDI Composites International/IDI SMC E-205 |
---|---|---|---|
dielectric strength | ASTM D149 | 14 kV/mm | |
arc resistance | ASTM D495 | >180 sec |
Mechanical properties | Test Condition | Test Method | IDI Composites International/IDI SMC E-205 |
---|---|---|---|
tensile strength | ASTM D638 | 96.5 MPa | |
compressive strength | ASTM D695 | 207 MPa | |
Flexural modulus | ASTM D790 | 12400 MPa | |
bending strength | ASTM D790 | 179 MPa |
flammability | Test Condition | Test Method | IDI Composites International/IDI SMC E-205 |
---|---|---|---|
UL flame retardant rating | 3.0mm | UL 94 | V-0 |
1.2mm | UL 94 | V-0 | |
1.5mm | UL 94 | V-0 |
physical property | Test Condition | Test Method | IDI Composites International/IDI SMC E-205 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.0to0.20 % |
ASTM D1895 | 1.0 | ||
Water absorption rate | 23°C,24hr | ASTM D570 | 0.11 % |
density | ASTM D792 | 1.70to1.90 g/cm³ |
Thermal performance | Test Condition | Test Method | IDI Composites International/IDI SMC E-205 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | >260 °C |