Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA46 TW241F3 DSM HOLAND
Stanyl®
Automotive Applications,Home appliance components
Thermal stability,Lubricity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DSM HOLAND/TW241F3 |
|---|---|---|---|
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 290 °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 275 °C | |
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 8.0E-5 cm/cm/°C |
| Flow | ISO 11359-2 | 5.0E-5 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 295 °C | |
| RTI Elec | 0.75 mm | UL 746 | 65.0 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/TW241F3 |
|---|---|---|---|
| Bending modulus | ISO 178 | 5800 Mpa | |
| Tensile modulus | 200°C | ISO 527-2 | 2350 Mpa |
| -- | ISO 527-2 | 6100 Mpa | |
| 120°C | ISO 527-2 | 3000 Mpa | |
| 160°C | ISO 527-2 | 2650 Mpa | |
| 180°C | ISO 527-2 | 2500 Mpa | |
| Tensile strain | Break, 180°C | ISO 527-2 | 12 % |
| Break, 160°C | ISO 527-2 | 12 % | |
| Break, 120°C | ISO 527-2 | 12 % | |
| Break | ISO 527-2 | 4.0 % | |
| Break, 200°C | ISO 527-2 | 12 % | |
| tensile strength | Break, 120°C | ISO 527-2 | 85.0 Mpa |
| Break, 200°C | ISO 527-2 | 65.0 Mpa | |
| Break | ISO 527-2 | 140 Mpa | |
| Break, 180°C | ISO 527-2 | 70.0 Mpa | |
| Break, 160°C | ISO 527-2 | 75.0 Mpa |
| Physical properties | Test Condition | Test Method | DSM HOLAND/TW241F3 |
|---|---|---|---|
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 3.2 % |
| impact performance | Test Condition | Test Method | DSM HOLAND/TW241F3 |
|---|---|---|---|
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 45 kJ/m² |
| 23°C | ISO 179/1eU | 50 kJ/m² |
| flammability | Test Condition | Test Method | DSM HOLAND/TW241F3 |
|---|---|---|---|
| Flammability level | UL 94 | HB |