Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Polyester, TS Glastherm® HT USA Glastic
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | USA Glastic/Glastherm® HT |
|---|---|---|---|
| Linear coefficient of thermal expansion | TD | ASTM D696 | 1.2E-04 cm/cm/°C |
| MD | ASTM D696 | 2.2E-05 cm/cm/°C | |
| thermal conductivity | ASTMC177 | 0.27 W/m/K |
| mechanical properties | Test Condition | Test Method | USA Glastic/Glastherm® HT |
|---|---|---|---|
| bending strength | Yield | ASTM D790 | 214 MPa |
| compressive strength | 200°C | ASTM D695 | 124 MPa |
| 288°C | ASTM D695 | 117 MPa | |
| 24°C | ASTM D695 | 338 MPa | |
| 150°C | ASTM D695 | 186 MPa |
| Electrical performance | Test Condition | Test Method | USA Glastic/Glastherm® HT |
|---|---|---|---|
| Dielectric strength | inAir | ASTM D149 | 2.0 kV/mm |
| Physical properties | Test Condition | Test Method | USA Glastic/Glastherm® HT |
|---|---|---|---|
| density | ASTM D792 | 1.97 g/cm³ | |
| Water absorption rate | 24hr | ASTM D570 | 0.20 % |
| impact performance | Test Condition | Test Method | USA Glastic/Glastherm® HT |
|---|---|---|---|
| Impact strength of cantilever beam gap | ASTM D256 | 430 J/m |
| flammability | Test Condition | Test Method | USA Glastic/Glastherm® HT |
|---|---|---|---|
| UL flame retardant rating | 23.9mm | UL 94 | HB |